固浪免砸砖
FREE BRICK
施工说明:
1、每组材料可施工5个平方以内,如正在漏水先停止使用水保持地面无水,等漏水排空后在使用本产品效果最佳。
2使用壁纸刀把地面瓷砖缝划开,划得越深施工效果越好。
3、施工前先堵住地漏、有排水的地方。
4、将本产品A料加入18公斤至20公斤清水以内搅拌完全溶解。
5、在加入B料固化剂,直接倒在厨卫浴地面,要求瓷砖地表面必须有1-2公分的材料,然后用扫帚从低处往高处扫,持续扫40-50分钟左右、扫动时间越长凝固时间延长,使堵漏胶均匀渗透。
6、材料完全固化后形成果冻透明胶体,用腻子刀或铲刀把瓷砖上残留胶体清理干净,即可,正常使用或者24小时后做蓄水测试
Construction instructions:
1. Each group of materials can be constructed within 5 square meters. If water is leaking, stop using water to keep the ground water-free. After using the water leakage, the best effect is to use this product.
2 Use the wallpaper knife to sew the floor tiles, the deeper the construction, the better the construction effect.
3. Block the floor drain and drainage before construction.
4. Add the A material of this product to the mixture of 18 kg to 20 kg of water to dissolve completely.
5, in the addition of B material curing agent, directly on the kitchen floor, the surface of the tile requires 1-2 cm of material, and then sweep from the low to the high with a broom, continue to sweep about 40-50 minutes, sweep The longer the moving time is, the longer the solidification time is, so that the plugging glue penetrates evenly.
6. After the material is completely cured, form a jelly transparent colloid. Clean the residual gel on the tile with a putty knife or a blade. Normally use or do a water storage test after 24 hours.
注意事项:
免砸砖的施工方法,按这个进行施工,
施工之前卫生间要控水两天,不要洗澡洗衣服,正常用没事
Precautions:
Construction method of free bricks, construction according to this,
Before the construction, the bathroom should be controlled for two days. Do not take a bath to wash clothes. Normal use is fine.
保质期:
原装密封产品在干燥阴凉的环境下存放。在正常的储存和运输条件下,产品的保质期为二年。
Shelf life:
The original sealed product is stored in a dry and cool environment. Under normal conditions of storage and transportation, the shelf life of the product is two years.
全国免费服务热线:400-843-6198